MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
ITW Devcon® Epoxy Concrete Sealer
Categories: Polymer; Thermoset; Epoxy

Material Notes: A 100% solids, two-component, self-leveling, non-voc clear epoxy sealer for sealing and water-proofing concrete, masonry, and wood surfaces. Uses: Ideal clear coating high traffic areas. A good primer for damp surfaces before applying a top coat. Features: Resists industrial chemicals, Applies with brush or roller, Bonds to damp surfaces, Applies at temperatures as low as 40°F.

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 100 %
Viscosity 2000 cPMixed
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 85
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 90.0 °F
Minimum Service Temperature, Air 40.0 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 24.0 hour
@Temperature 24.0 °C
Foot Traffic
 24.0 hour
@Temperature 24.0 °C
Functional cure
 72.0 hour
@Temperature 24.0 °C
Full service
 168 hour
@Temperature 24.0 °C
As Tested
Pot Life 60.0 min
@Temperature 23.9 °C
 
Descriptive Properties
Chemical/Solvent Resistance1,1,1-Trichloroethane: excellent30 day immersion at 75°F. Sample cured 7 days at RT
 Ammonium Hydroxide 20%: very good30 day immersion at 75°F. Sample cured 7 days at RT
 Cutting oil: very good30 day immersion at 75°F. Sample cured 7 days at RT
 Gasoline (unleaded): very good30 day immersion at 75°F. Sample cured 7 days at RT
 Hydrochloric 36%: poor30 day immersion at 75°F. Sample cured 7 days at RT
 Hydrochloric Acid 10%: very good30 day immersion at 75°F. Sample cured 7 days at RT
 Methanol: poor30 day immersion at 75°F. Sample cured 7 days at RT
 Methyl Ethyl Ketone: poor30 day immersion at 75°F. Sample cured 7 days at RT
 Methylene Chloride: very good30 day immersion at 75°F. Sample cured 7 days at RT
 Phosphoric 50%: poor30 day immersion at 75°F. Sample cured 7 days at RT
 Phosphoric Acid 10%: very good30 day immersion at 75°F. Sample cured 7 days at RT
 Potassium Hydroxide 40%: excellent30 day immersion at 75°F. Sample cured 7 days at RT
 Sodium Hydroxide 50%: excellent30 day immersion at 75°F. Sample cured 7 days at RT
 Sodium Hypochlorite: very good30 day immersion at 75°F. Sample cured 7 days at RT
 Sulfuric 50%: poor30 day immersion at 75°F. Sample cured 7 days at RT
 Sulfuric Acid 10%: very good30 day immersion at 75°F. Sample cured 7 days at RT
ColorclearCured
Coverage400 ft²Cured. @ 8 mils
Mix Ratio by volume2.2:1
Mix Ratio by weight2.8:1
Recoat Time8 to 10 hrs

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PITWD9219 / 239728

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.