MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Hanwha Azdel Plus U400-B01N 41.5% Directionalized Continuous Fiber Mat / PP Resin Matrix
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: AZDEL® U400-B01N is a uni-directional fiber and random glass mat reinforced polypropylene composite material featuring excellent fiber distribution over long flow paths and complex part forms. This material allows highly directionalized reinforcement where loads are in defined planes.

Typically it is combined with Azdel chopped and random mat to localized high stress paths, minimizing part weight and cost. For use in semi-structural applications and especially suited to adhesion bonded assemblies.

Commercially available only to European based customers.

Information provided by Azdel.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.24 g/ccISO 1183
Filler Content 41.5 %ISO 1172
Thickness 3200 micronsAZDEL Test
Linear Mold Shrinkage, Flow 0.0020 cm/cmflat plaques, 320 x 320 mm; ISO 2577
Linear Mold Shrinkage, Transverse 0.0040 cm/cmmeasured on flat plaques, 320 x 320 mm; ISO 2577
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 80.0 MPaTransverse direction; ISO 527/4
 250 MPaLongitudinal direction; ISO 527/4
Elongation at Break 2.0 %Transverse direction; ISO 527/4
 2.3 %Longitudinal direction; ISO 527/4
Tensile Modulus 5.80 GPaTransverse direction; ISO 527/4
 9.30 GPaLongitudinal direction; ISO 527/4
Flexural Strength 130 MPaTransverse direction; ISO 178
 250 MPaLongitudinal direction; ISO 178
Flexural Modulus 5.50 GPaTransverse direction; ISO 178
 8.00 GPaLongitudinal direction; ISO 178
Charpy Impact, Notched 6.50 J/cm²Transverse direction; ISO 179/2fn
 14.0 J/cm²Longitudinal direction; ISO 179/2fn

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Envalior TEPEX® dynalite 104-RG600(x)/47% Roving Glass – PP Consolidated Composite Laminate
Akro-Plastic Akromid® A3 GF 30 1 L natural (4715) PA66 + PP, Dry, 30% Glass Filled
Niche Polymer POLIXL™ PA66GF33N PA66, 33% Fiberglass Reinforced, DAM
Domo TECHNYL® C 216 V35 Black Z PA6, 35% glass fiber, DRY
Celanese Celstran® PP-GF30-04 natural PP, 30% Glass Reinforced

PZZGEAZ80 / 40629

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.