For economical molding products; Economical grade for keypads or parts C-8 & C-8E: Properties obtained using 2% curing agent on 2mm thick slabs, cured 5 minutes at 170°C. C15 & C-8BS: Properties obtained using 2% curing agent on 2mm thick slabs, cured 10 minutes at 170°C. LSR: Mixed part A and part B first, cured 5 minutes at 130°C. All physical properties are obtained from first cured samples. Curing Agent C-8, C-8BS, C-15, C-8E are 2,5-Bis(tert-butylperoxy)-2,5-dimethylhexane paste. C-8 is normal type. C-15 is anti-yellowing type. C-8E is flame-retardant type. Information provided by SiSiB Silicones - PCC Group |