MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Latrobe Lescalloy® 300M VAC-ARC High Strength Alloy Steel
Categories: Metal; Ferrous Metal; Alloy Steel; Carbon Steel; High Carbon Steel

Material Notes: LESCALLOY 300M VAC-ARC steel is a modified 4340 steel with added silicon allowing for use of a higher tempering temperature. The steel has high hardenability and strength with good ductility and toughness in heavy sections. It is used primarily in the 270/300 ksi (1862/2068) tensile strength range for aircraft landing gears, flap tracks and other structural applications. Vacuum arc remelting (VAR) is used to provide optimum cleanliness and preferred ingot structure.

Information Provided by Timken Latrobe Steel.

Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 7.83 g/cc0.283 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C 57.557.51" from quench end; Jominy End Quench Hardenability
 58581/2" from quenched end; Jominy End Quench Hardenability
 59591/8" from quenched end; Jominy End Quench Hardenability
Tensile Strength, Ultimate 1970 - 1990 MPa286000 - 288000 psi302°C Temper Temperature
Tensile Strength, Yield 1655 - 1689 MPa
@Strain 0.2 %
240000 - 245000 psi
@Strain 0.2 %
302°C Temper Temperature
Elongation at Break 8.5 - 11 %8.5 - 11 %302°C Temper Temperature
Reduction of Area 31 - 39 %31 - 39 %302°C Temper Temperature
 
Thermal PropertiesMetricEnglishComments
CTE, linear 11.34 µm/m-°C
@Temperature -17.8 - 93.0 °C
6.300 µin/in-°F
@Temperature -0.0400 - 199 °F
Specific Heat Capacity 0.448 J/g-°C0.107 BTU/lb-°F
Thermal Conductivity 37.49 W/m-K260.2 BTU-in/hr-ft²-°F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.42 %0.42 %
Chromium, Cr 0.80 %0.80 %
Iron, Fe 94.11 %94.11 %
Manganese, Mn 0.75 %0.75 %
Molybdenum, Mo 0.40 %0.40 %
Nickel, Ni 1.8 %1.8 %
Silicon, Si 1.65 %1.65 %
Vanadium, V 0.070 %0.070 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
300M Ultrahigh Strength Steel
Latrobe Lescalloy® 300M - HS VAC-ARC High Strength Alloy Steel
Latrobe Lescalloy® 4340 VAC-ARC ; 3.5" round High Strength Alloy Steel
Latrobe Lescalloy® 9310 VAC-ARC Premium Carburizing Steel
ATI Allvac® Vasco® 9310 Specialty Steel, Heat Treatment: 899°C (1650°F) Normalization

NTIMK017 / 19365

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.