MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil Enable™ 27-05HH Metallocene Polyethylene Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Product Description: Enable 27-05HH is a metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact and puncture. Easier processing and excellent properties lead to significant high pressure LDPE replacement in many applications, yet with superior drawdown and enhanced toughness.

Availability: Latin America, North America and South America

Additive:

  • Antiblock: No
  • Slip: No
  • Processing Aid: Yes
  • Thermal Stabilizer: Yes
Applications:
  • Blown Film
  • Collation Shrink
  • Food packaging
  • Form Fill and Seal Packaging
  • Heavy Duty Bags
  • Lamination Film
  • Multilayer Packaging Film
  • Shrink Film
  • Stand Up Pouches

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.927 g/ccExxonMobil method
Melt Flow 0.50 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 1900 psiASTM D882
Film Tensile Strength at Yield, TD 2100 psiASTM D882
Film Elongation at Break, MD 520 %ASTM D882
Film Elongation at Break, TD 770 %ASTM D882
Puncture Energy 25.0 in-lbExxonMobil Method
Elmendorf Tear Strength MD 50 gASTM D1922
Elmendorf Tear Strength TD 730 gASTM D1922
Dart Drop Test 130 gASTM D1709A
Film Tensile Strength at Break, MD 8500 psiASTM D882
Film Tensile Strength at Break, TD 7300 psiASTM D882
1% Secant Modulus, MD 43000 psiASTM D882
1% Secant Modulus, TD 51000 psiASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point <= 246 °FPeak Melting Point; ExxonMobil method
 
Optical PropertiesOriginal ValueComments
Haze 11 %ASTM D1003
Gloss 49 %45°; ASTM D2457
 
Descriptive Properties
Puncture Force11 lbfExxonMobil Method

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil Enable™ 20-05HH Metallocene Polyethylene Resin
ExxonMobil Enable™ 23-05HH Metallocene Polyethylene Resin
ExxonMobil Enable™ 20-10HE Metallocene Polyethylene Resin
ExxonMobil Enable™ 35-05HH Metallocene Polyethylene Resin
ExxonMobil Exceed™ 1018KA Metallocene Polyethylene Resin

PEX99010 / 175247

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.