MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
LyondellBasell Petrothene HR52811E Linear Medium Density Polyethylene (LMDPE), Film
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Medium Density (MDPE); Linear Medium Density Polyethylene (LMDPE), Film

Material Notes: Petrothene HR52811E is a high performance, linear polyethylene grade with medium density and hexene as comonomer designed for use in jacketing, conduit or wire insulation. This product exhibits an excellent ESCR and a high impact strength at low temperatures. Petrothene HR52811E contains a robust additives package for thermal stabilization, UV stabilizers and a processing aid. The product is delivered in pellet form and meets the requirements of ASTM D 1248, Type II, Class A, Category 4, Grade J5. Applications: Wire & Cable

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.9636 g/ccISO 1183-1
Environmental Stress Crack Resistance >= 5000 hourASTM D 1693
Oxidative Induction Time (OIT) >= 60 min
@Temperature 200 °C
ISO 11357-6
Melt Flow 0.75 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133-1
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 57ISO 868
Tensile Strength at Break 28.0 MPaISO 527-1,-2
Tensile Strength, Yield 16.0 MPaISO 527-1,-2
Elongation at Break >= 500 %ISO 527-1,-2
Tensile Modulus 600 MPaISO 527-1,-2
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+17 ohm-cmIEC 93
Dielectric Constant 2.3IEC 250
Dielectric Strength 1370 V/milIEC 60243-1
Dissipation Factor <= 0.0010
 
Thermal PropertiesOriginal ValueComments
Melting Point 126 °Cpeak; ISO 3146
Vicat Softening Point 119 °CA/50N; ISO 306
 
Descriptive Properties
FNCT (hrs)>1000ISO 16770, 4.0 MPa, 2% Arkopal N100, 80°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Novolen® 3300 MC Polypropylene
BASF Novolen® 2700 L Polypropylene
ScanTube FEP Tubing
ScanTube MFA Tubing
ScanTube PFA Tubing

PEQT8833 / 220467

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.