MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Extreme Materials from MCAM
Visit Mitsubishi Chemical Advanced Materials for Extreme Materials - high performance plastic machining stock engineered to replace metals such as nickel alloys or stainless steel.

MetalTek MTEK CX-2MW Cast UNS N26022 Severe Corrosion and Heat Resistant Alloy
Categories: Metal; Nonferrous Metal; Nickel Alloy; Superalloy

Material Notes: Information provided by MetalTek

Key Words: Cast UNS N26022; Cast Grade CX-2MW; Cast ASTM A494; Wrought UNS N06022; Wrought Grade HASTELLOY® C-22
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate >= 550 MPa>= 79800 psi
Tensile Strength, Yield >= 310 MPa>= 45000 psi
Elongation at Break >= 30 %>= 30 %
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.020 %<= 0.020 %
Chromium, Cr 20 - 22.5 %20 - 22.5 %
Iron, Fe 2.0 - 6.0 %2.0 - 6.0 %
Manganese, Mn <= 0.80 %<= 0.80 %
Molybdenum, Mo 12.5 - 14.5 %12.5 - 14.5 %
Nickel, Ni 51.33 - 63 %51.33 - 63 %As Balance
Silicon, Si <= 1.0 %<= 1.0 %
Tungsten, W 2.5 - 3.5 %2.5 - 3.5 %
Vanadium, V <= 0.35 %<= 0.35 %
 
Descriptive Properties
Heat TreatmentSol. Anneal

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
MetalTek MTEK CW-12MW Cast UNS N30002 Severe Corrosion and Heat Resistant Alloy
MetalTek MTEK N-7M Cast UNS N30007 Severe Corrosion and Heat Resistant Alloy
Haynes Hastelloy® C-22® alloy, 12.7-50.8 mm thick bar, solution heat treated
MetalTek MTEK CW-2M Cast UNS N26455 Severe Corrosion and Heat Resistant Alloy
ATI Allvac® Nickelvac® C 22 UNS N06022 Nickel Superalloy

NMETEK127 / 18377

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.