MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Röhm ACRYLITE® H15 Acrylic Polymer
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, Extruded; Acrylic, General Purpose, Molded

Material Notes: ACRYLITE® H15 acrylic polymer is an amorphous thermoplastic molding and extrusion compound based on polymethyl methacrylate (PMMA).

Typical properties of ACRYLITE® acrylic polymers are excellent weather resistance, high light transmission, high mechanical strength, high surface hardness and mar resistance, good melt flow rate, and versatile colorability due to crystal clarity.

The special properties of ACRYLITE H15 polymer are medium heat resistance, high melt strength, UV light absorption options, lubricant options, and AMECA listed.

Application: Used for injection molding and extrusion of optical and technical parts.

Information Provided by Evonik CYRO. The former Evonik Methacrylates business has been sold to Röhm (Roehm) GmbH.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.19 g/ccASTM D792
Bulk Density 0.660 g/ccASTM D1895
Water Absorption at Saturation 0.30 %ASTM D570
Linear Mold Shrinkage 0.0040 - 0.0070 in/inASTM D955
Melt Flow 2.2 g/10 min
@Load 3.80 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 95ASTM D785
Tensile Strength at Break 9800 psiASTM D638
Elongation at Break 4.0 - 6.0 %ASTM D638
Elongation at Yield 4.0 - 6.0 %ASTM D638
Tensile Modulus 470000 psiASTM D638
Flexural Strength 17000 psiASTM D790
Flexural Modulus 490000 psiASTM D790
Izod Impact, Notched 0.360 ft-lb/in
@Temperature 23.0 °C
1/4" bar; ASTM D256
 
Thermal PropertiesOriginal ValueComments
CTE, linear 72.0 µm/m-°C
@Temperature 0.000 - 100 °C
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 203 °F
@Thickness 6.35 mm
Annealed; ASTM D648
Vicat Softening Point 221 °FASTM D1525
 
Optical PropertiesOriginal ValueComments
Haze <= 1.0 %ASTM D1003
Yellow Index <= 1.0 %ASTM D1925
Transmission, Visible 92 %ASTM D1003
 
Processing PropertiesOriginal ValueComments
Middle Barrel Temperature 460 - 480 °F
Melt Temperature 460 - 480 °F
Mold Temperature 90.0 - 175 °F
Drying Temperature 175 °F
Dry Time 3 - 4 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LG Chemical IH830A PMMA, General Purpose Grade for Injection Molding
Röhm Acrylite® 8N Acrylic Polymer
Röhm Acrylite® H15 Compound Molding and Extrusion
Trinseo Plexiglas® V826 Acrylic
Röhm Acrylite Plus® zdf Impact Acrylic Polymer

PCYR00050 / 101039

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.