MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Torlon® 4203L PAI, General purpose
Categories: Polymer; Thermoplastic; Polyamide-imide (PAI)

Material Notes: General purpose, unfilled, best impact resistance, most elongation, good mold release, good electrical properties

Torlon® 4203L is an unreinforced, lubricated, pigmented grade of polyamide-imide (PAI) resin. It has the best impact resistance and greatest elongation of all the Torlon® grades. Torlon® PAI has the highest strength and stiffness of any thermoplastic up to 275°C (525°F). It has outstanding resistance to wear, creep, and chemicals.

Torlon® 4203L resin offers outstanding electrical properties, which makes it ideal for high performance parts such as connectors, switches and relays. In addition Torlon® 4203L polyamide-imide can be used in applications such as thrust washers, spline liners, valve seats, bushings, bearings, wear rings, cams and other applications requiring strength at high temperature and resistance to wear.

- High Flow: Torlon® 4203L-HF
- Low Flow: Torlon® 4203L-LF

Applications: Aircraft Applications; Automotive Applications; Bushings; Connectors; Electrical Parts; Electrical/Electronic Applications; Fasteners; Film; Machine/Mechanical Parts; Oil/Gas Applications; Semiconductor Molding Compounds; Thrust Washer

Features: Chemical Resistant; Creep Resistant; Ductile; Fatigue Resistant; Flame Retardant; Good Electrical Properties; High Heat Resistance; High Temperature Strength; Low Temperature Toughness; Ultra High Impact Resistance; Wear Resistant

Information provided by Solvay Specialty Polymers.

Vendors: Drake extrudes shapes and machines and injection molds parts in Torlon® PAI, PEEK, PAEK, Ryton PPS and Ultem PEI. It also machines Vespel® PI. Innovations include cryogenic CryoDyn® CT-200 shapes as a PCTFE alternative; efficient Seamless Tube® and the largest extruded rod diameters to >254mm and plate thicknesses to > 100mm. Certified to ISO 9001:2015 and AS9100D. Visit www.DrakePlastics.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.42 g/ccASTM D792
Water Absorption 0.33 %
@Time 86400 sec
ASTM D570
Linear Mold Shrinkage, Flow 0.0060 - 0.0085 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 152 MPaType I; ASTM D638
Tensile Stress 192 MPaASTM D1708
Elongation at Break 7.6 %Type I; ASTM D638
Tensile Modulus 4480 MPaType I; ASTM D638
Flexural Strength 118 MPa
@Temperature 232 °C
ASTM D790
 241 MPa
@Temperature 23.0 °C
ASTM D790
Flexural Modulus 3590 MPa
@Temperature 232 °C
ASTM D790
 5030 MPa
@Temperature 23.0 °C
ASTM D790
Compressive Strength 221 MPaASTM D695
Compressive Modulus 4000 MPaASTM D695
Poissons Ratio 0.45ASTM E132
Izod Impact, Notched 140 J/mASTM D256
Izod Impact, Unnotched 1100 J/mASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 2.00e+17 ohm-cmASTM D257
Surface Resistance 5.00e+18 ohmASTM D257
Dielectric Constant 3.9
@Frequency 1e+6 Hz
ASTM D150
 4.2
@Frequency 60 Hz
ASTM D150
Dielectric Strength 23.0 kV/mmASTM D149
Dissipation Factor 0.026
@Frequency 60 Hz
ASTM D150
 0.031
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 31.0 µm/m-°CASTM E831
Thermal Conductivity 0.260 W/m-KASTM C177
Deflection Temperature at 1.8 MPa (264 psi) 278 °CUnannealed; ASTM D648
Glass Transition Temp, Tg 277 °CISO 11357-2
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 304 °C
Nozzle Temperature 371 °C
Mold Temperature 199 - 216 °C
Drying Temperature 177 °C
@Time 10800 sec
Moisture Content <= 0.050 %Injection
Back Pressure 6.89 MPa
Screw Speed 50 - 100 rpm
 
Descriptive Properties
AdditivePTFE Lubricant
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
FormsPellets
ProcessingInjection Molding; Machining; Profile Extrusion
RoHS ComplianceYes
Screw L/D Ratio, Injection18.0:1.0 to 24.0:1.0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOL8Y4545 / 280345

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.