Escorene Ultra LD 767.MJ is a high viscosity, 29.5% vinyl acetate copolymer suitable for making very soft, blow molded or extruded articles with very good low temperature toughness. It can also be used as a polymer modifier to make specialty compounds. Information provided by ExxonMobil Chemical |