MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Teknor Apex Monprene® RG-28163 CLR XRD1 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Monprene RG-28163 CLR XRD1 is a high performance thermoplastic elastomer designed for consumer and industrial applications, including food contact, film and tubing. Monprene RG-28163 CLR XRD1 is a medium hardness, low density, RoHS compliant grade with excellent adhesion to PP. This grade is suitable for cast film and extrusion.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: Chemical Resistant; Good Adhesion; Good Colorability; Good Melt Strength; Good Processability; Good Toughness; Halogen Free; High Clarity; High Purity; Kink Resistant; Low Density; Low Specific Gravity; Lubricated; Medium Hardness

Uses: Clear Sheet; Film; Food Service Applications; Hose; Non-specific Food Applications; Tubing

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Extrusion; Cast Film

Preliminary data. Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.890 g/cc0.0322 lb/in³ASTM D792
Water Vapor Transmission  1.29 g/m²/day
@Thickness 1.02 mm,
Temperature 37.8 °C
0.0830 g/100 in²/day
@Thickness 0.0400 in,
Temperature 100 °F
100% RH; ASTM F1249
 51.2 g/m²/day
@Thickness 0.0254 mm,
Temperature 37.8 °C
3.30 g/100 in²/day
@Thickness 0.00100 in,
Temperature 100 °F
100% RH; ASTM F1249
Oxygen Transmission  12.5 cc-mm/m²-24hr-atm
@Thickness 1.02 mm
31.7 cc-mil/100 in²-24hr-atm
@Thickness 0.0400 in
90% RH, Wet; ASTM F1927
 13.1 cc-mm/m²-24hr-atm
@Thickness 1.02 mm
33.2 cc-mil/100 in²-24hr-atm
@Thickness 0.0400 in
35% RH, Wet; ASTM F1927
Melt Flow 4.5 g/10 min
@Load 5.00 kg,
Temperature 200 °C
4.5 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A  65
@Time 5.00 sec
65
@Time 0.00139 hour
Injection Molded; ASTM D2240
 67
@Time 1.00 sec
67
@Time 0.000278 hour
Injection Molded; ASTM D2240
Tensile Strength at Break 11.9 MPa1720 psiDie C, 20 in/min; ASTM D412
Tensile Stress at Strain  2.24 MPa
@Strain 50 %
325 psi
@Strain 50 %
Die C, 20 in/min; ASTM D412
 2.65 MPa
@Strain 100 %
385 psi
@Strain 100 %
Die C, 20 in/min; ASTM D412
 4.24 MPa
@Strain 300 %
615 psi
@Strain 300 %
Die C, 20 in/min; ASTM D412
Elongation at Break 630 %630 %Die C, 20 in/min; ASTM D412
Tear Strength 43.3 kN/m247 pliDie C, 20 in/min; ASTM D624
Compression Set  18 %
@Temperature 22.8 °C,
Time 79200 sec
18 %
@Temperature 73.0 °F,
Time 22.0 hour
Type 1; ASTM D395B
 86 %
@Temperature 70.0 °C,
Time 79200 sec
86 %
@Temperature 158 °F,
Time 22.0 hour
Type 1; ASTM D395B
 
Processing PropertiesMetricEnglishComments
Zone 1 160 - 177 °C320 - 350 °F
Zone 2 171 - 191 °C340 - 375 °F
Zone 3 182 - 204 °C360 - 400 °F
Zone 4 182 - 204 °C360 - 400 °F
Zone 5 182 - 210 °C360 - 410 °F
Die Temperature 177 - 216 °C350 - 420 °F
Screw Speed 30 - 100 rpm30 - 100 rpm
 
Descriptive Properties
AppearanceClear/Transparent
 Colors Available

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTEKNQ0947 / 237438

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.