MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Covestro Bayflex® XGT-15 Polyurethane System, Unfilled
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Solid RIM

Material Notes: Characterization: Bayflex XGT-15 is an elastomeric polyurethane system used in the reaction injection molding (RIM) process.

Properties / Applications: Bayflex XGT-15 is an elastomeric polyurethane system used in the reaction injection molding (RIM) process. The formulated system is supplied as two liquid components: Component A is a diphenylmethane diisocyanate (MDI) prepolymer, and Component B is a polyether polyol system. Bayflex XGT-15 system has a flexural modulus of 16,00 psi* at room temperature. It is used in applications requiring long shot times allowing large parts to be made on smaller equipment. The Bayflex XGT-15 system is suitable for use in glass encapsulation applications, or in applications requiring excellent impact properties, such as bus and truck bumpers or equipment housings. As with any product, use of the Bayflex XGT-15 system in a given application must be tested (including field testing, etc.) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.04 g/ccPolyol (Component B)
 1.04 g/ccASTM D792
 1.21 g/ccIsocyanate (Component A)
Viscosity 700 cPIsocyanate (Component A)
 1200 cPPolyol (Component B)
Linear Mold Shrinkage 0.0080 - 0.0090 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 94ASTM D2240
Hardness, Shore D 45ASTM D2240
Tensile Strength at Break 16.5 MPaASTM D412
Elongation at Break 250 %ASTM D412
Flexural Modulus 110 MPaASTM D790
Tear Strength 450 pliDie C; ASTM D624
Taber Abrasion, mg/1000 Cycles 200
@Load 1.00 kg
H-18 Wheel; ASTM D3489
 
Thermal PropertiesOriginal ValueComments
CTE, linear 78.0 µin/in-°FASTM D696
Flash Point 114 °CPolyol (Component B)
 213 °CIsocyanate (Component A)
 
Processing PropertiesOriginal ValueComments
Mold Temperature 60.0 - 70.0 °C
 
Descriptive Properties
AppearanceColorless to pale yellow liquidPolyol (Component B)
 Light yellow to yellow liquidIsocyanate (Component A)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Alliance Polymers Zythane™ 7090A Thermoplastic Polyurethane Elastomer
Covestro Bayflex® LSR 10 Elastomer
Covestro Bayflex® MP-10000 Polyurethane Elastomeric RIM, MDI-based 2-Component Liquid System
Covestro Bayflex® XGT-16 Polyurethane Elastomeric RIM, MDI-based 2-Component Liquid System
Covestro Baytec® ME-120 Polyurethane

PCOVEST0140 / 201923

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.