MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SABIC LNP™ THERMOCOMP™ Compound LC004XXP Polyetheretherketone (PEEK)
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK)

Material Notes: LNP THERMOCOMP LC004XXP compound is based on Polyetheretherketone (PEEK) resin containing 20% carbon fiber. Added features of this grade include: Electrically Conductive.

Features: High Stiffness,Light-weight Structural,High Heat Resistance,Super Strong (Carbon Fiber Filled),Electrically Conductive,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.36 g/cc0.0491 lb/in³ISO 1183
Moisture Absorption 0.100 %0.100 %Injection Molding
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm0.0010 - 0.0030 in/inSABIC method
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 199 MPa28900 psi5 mm/min; ISO 527
Elongation at Break 1.9 %1.9 %5 mm/min; ISO 527
Flexural Strength 280 MPa40600 psiyield, 2 mm/min; ISO 178
Flexural Modulus 13.9 GPa2020 ksi2 mm/min; ISO 178
Izod Impact, Notched (ISO) 10.0 kJ/m²4.76 ft-lb/in²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 45.0 kJ/m²21.4 ft-lb/in²80*10*4; ISO 180/1U
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 100 - 10000 ohm100 - 10000 ohmASTM D257
 
Processing PropertiesMetricEnglishComments
Zone 2 365 - 375 °C689 - 707 °F
Zone 3 380 - 395 °C716 - 743 °F
Melt Temperature 380 - 390 °C716 - 734 °FInjection Molding
Mold Temperature 140 - 165 °C284 - 329 °F
Drying Temperature 120 - 150 °C248 - 302 °FInjection Molding
Dry Time 4.00 hour4.00 hourInjection Molding
Back Pressure 0.300 - 0.700 MPa43.5 - 102 psi
Screw Speed 60 - 100 rpm60 - 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH81666 / 289613

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.