MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Hexcel® HexTow® AS7 Carbon Fiber - Epoxy Composite
Categories: Polymer; Thermoset; Carbon Fiber/Thermoset Composite; Epoxy; Epoxy/Carbon Fiber Composite

Material Notes: HexTow™ AS7 carbon fiber is a continuous, high strength, high strain, PAN based fiber available, in a 12,000 (12K) filament count tow. This fiber has been surface treated and can be sized to improve its interlaminar shear properties, handling characteristics, and structural properties. Suggested for use in prepregging, weaving, and filament winding.

Property data data for a typical 62 vol% epoxy composite

Information provided by Hexcel

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Filler Content 62.0 %Fiber Volume
Filament Diameter 6.9 µm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 2415 MPa
Tensile Modulus 152 GPa
Flexural Modulus 128 GPa
Shear Strength 124 MPashort-beam
 
Descriptive Properties
Tow Cross-Sectional Area (mm2)0.4512K

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
TIMET 6-6-2 Titanium Alloy (Ti-6Al-6V-2Sn), Solution Treated and Aged
AISI Grade 18Ni (350) Maraging Steel, Aged, at RT, tested transverse, sheet 6 mm thick
Hexcel® HexTow® AS4D Carbon Fiber - Epoxy Composite
AISI Type S14800 Stainless Steel condition CH900, 72.5% cold reduction
Carpenter Vega® Alloy Tool Steel (Air-Tough) (AISI A6)

PHEXC677 / 230542

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.