MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Kohesi Bond TUF 1828 TC One component, toughened, low thermal resistance epoxy
Categories: Polymer; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Product Highlights:
  • Unrivaled heat transfer efficiency
  • Cryogenic service
  • Superb mechanical strength properties
  • Microns thin bond lines achievable
  • Capable of passing NASA low outgassing
  • Unlimited working life at room temperature
Kohesi Bond TUF 1828 TC is a toughened, single component, thermal management epoxy system that offers an unlimited working life at room temperature. This product has very low thermal resistance and can be applied in layers as thin as 10 microns. The efficiency of heat transfer improves exceedingly with lower thermal resistance. Since TUF 1828 TC can be applied in 10 micron thick sections, it offers a notably low thermal resistance of 5 - 6 × 10-6 m2•K/W. Being a one component system, it provides ease of application and also adheres well to a wide variety of substrates including metals, ceramics, composites, most plastics and glass. It provides superior bonding and physical strength properties. It has a gray color. Owing to its sensational thermal management properties and low outgassing properties TUF 1828 TC is widely used in electronics, optical, aerospace, specialty OEM and cryogenic industries.

Typical Applications:

  • Bonding
  • Sealing

Information provided by Kohesi Bond Custom Engineered Adhesives

Vendors: Kohesi Bond is a pioneer in manufacturing over 300 grades of custom engineered adhesives, sealants, coatings, potting and encapsulation compounds. Our first-rate adhesives are tailor-fitted to meet your exact specifications and offer superior strength and performance in your application. Learn more about Kohesi Bond’s industry-ready products at kohesibond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D >= 85>= 85
Tensile Strength >= 48.3 MPa>= 7000 psi
Compressive Strength >= 159 MPa>= 23000 psi
Adhesive Bond Strength >= 15.9 MPa>= 2300 psiTensile Lap Shear, Al/Al
Peel Strength 0.877 - 1.75 kN/m5.00 - 10.0 pliAl/Al
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 4.81
@Frequency 60 Hz
4.81
@Frequency 60 Hz
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 3.40 - 3.60 W/m-K23.6 - 25.0 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 200 °C392 °F
Minimum Service Temperature, Air -269 °C-452 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  60.0 - 90.0 min
@Temperature 120 - 150 °C
1.00 - 1.50 hour
@Temperature 248 - 302 °F
 120 - 240 min
@Temperature 180 °C
2.00 - 4.00 hour
@Temperature 356 °F
Post Cure
Shelf Life 3.00 - 6.00 Month3.00 - 6.00 Monthin original unopened containers
 
Descriptive Properties
Thermal Resistance5 - 6 × 10-6 m2·K/W
ViscositySmooth Paste

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PKOHESI992 / 249171

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.