Product Description: A soft, black thermoplastic vulcanizate, TPV (EPDM/PP) in the thermoplastic elastomer family which offers higher temperature resistance and excellent compression set with superior UV resistance. The Bondable to: PP, EVA, PE Availability: Africa & Middle East; Asia Pacific; Europe; North America Features: Bondability; Good Compression Set; High Heat Resistant; Soft; UV Resistant RoHS Compliance: RoHS Compliant Appearance: Black Forms: Pellets Processing Method: Injection Molding; ExtrusionInformation provided by Elastron |