MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Kraiburg TPE THERMOLAST® K TC4FRN Thermoplastic Elastomer (FR1 Series) Flame Retardant
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Material Notes: The FR1 series is a material solution for applications with flame retardant requirements. The compounds are halogen-free according to IEC 61249-2-21. The UL94 V-0 (3.0 mm) certificate is valid for available hardness range and for natural and colored compounds.

Processing Method: Injection Molding, Extrusion

Color / RAL DESIGN:

  • Natural
  • Black
Typical applications:
  • Gaskets for electric and electronic applications e.g. cable boxes
  • Gaskets for fire safety doors
  • Cable management systems e.g. cable holders, cable glands and grommets
Material advantages:
  • Halogen-free (according to IEC 61249-2-21)
  • Self-extinguishing, no release of burning droplets
  • Adhesion to PP
  • In-process recycling possible
  • Precoloration in all colors
  • Temperature stability up to 85 °C
  • High glow-wire flammability index (GWFI)
  • Stability in conditions up to 60 °C and 75% humidity

Information provided by Kraiburg TPE

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.13 g/ccDIN EN ISO 1183-1
Storage Temperature 15.0 - 30.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 37DIN ISO 48-4
Tensile Strength 2.00 MPa200 mm/min; DIN 53504/ISO 37
Elongation at Break 550 %200 mm/min; DIN 53504/ISO 37
Tear Strength 13.0 kN/mISO 34-1 Method B (b)
Compression Set 9.0 %
@Temperature 23.0 °C,
Time 259000 sec
DIN ISO 815-1 Method A
 30 %
@Temperature 70.0 °C,
Time 86400 sec
DIN ISO 815-1 Method A
 
Descriptive Properties
ColorNatural

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PKRAIA8247 / 308911

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.