MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Huntsman IROGRAN® A 92 H 4656 Polyester-Based TPU-Injection Molding Grade
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane TPE; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Polyester Grade

Material Notes: Introduction: IROGRAN A 92 H 4656 is a thermoplastic polyester- polyurethane for injection molding applications. Additional characteristics of the product are short cycle times, good melt flow and easy demolding.

Performance Features:

  • Good melt flow
  • Easy demolding
  • Short cycle times
  • Easy coloring recyclable
Applications: For the production of technical parts, wheels and rollers, cover plates, coupling halves, conveyor rollers

Information provided by Huntsman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.21 g/cc0.0437 lb/in³ASTM D792
Linear Mold Shrinkage 0.0060 cm/cm0.0060 in/inASTM D995
Melt Index of Compound 90 g/10 min
@Load 10.0 kg,
Temperature 210 °C
90 g/10 min
@Load 22.0 lb,
Temperature 410 °F
cm3/10 min
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9393ASTM D2240
Hardness, Shore D 4040ASTM D2240
Tensile Strength at Break 45.0 MPa6530 psiDIN 53504
Elongation at Break 740 %740 %ASTM D412
100% Modulus 8.90 MPa
@Strain 100 %
1290 psi
@Strain 100 %
DIN 53504
300% Modulus 18.6 MPa
@Strain 300 %
2700 psi
@Strain 300 %
DIN 53504
Rebound 32 %32 %Bayshore; ASTM D2632
Tear Strength 135 kN/m770 pliASTM D624
Abrasion 3030[mm3]; ISO 4649
Compression Set  25 %
@Temperature 23.0 °C,
Time 252000 sec
25 %
@Temperature 73.4 °F,
Time 70.0 hour
ASTM D395
 43 %
@Temperature 70.0 °C,
Time 86400 sec
43 %
@Temperature 158 °F,
Time 24.0 hour
ASTM D395
 
Thermal PropertiesMetricEnglishComments
Melting Point 170 - 185 °C338 - 365 °FHuntsman/TMA
 
Processing PropertiesMetricEnglishComments
Feed Temperature 25.0 - 40.0 °C77.0 - 104 °FExtrusion
Front Barrel Temperature 165 - 190 °C329 - 374 °FExtrusion
Nozzle Temperature 170 - 200 °C338 - 392 °FExtrusion
 180 - 200 °C356 - 392 °FInjection
Adapter Temperature 175 - 195 °C347 - 383 °FExtrusion
Die Temperature 175 - 200 °C347 - 392 °FExtrusion
Melt Temperature 170 - 195 °C338 - 383 °FInjection
Mold Temperature 20.0 - 70.0 °C68.0 - 158 °FInjection
 
Descriptive Properties
Heating Zone175-195°CInjection

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Alliance Polymers Zythane™ 3045D Thermoplastic Polyurethane Elastomer
Alliance Polymers Zythane™ 7090A Thermoplastic Polyurethane Elastomer
Barlog Plastics KEBAFLEX U A 85 HT B01 natural TPU, Shore A85, natural, high temperature resistance
Barlog Plastics KEBAFLEX U A 85 EF B01 natural TPU, Shore A85, natural, easy flow
Dow Prevail® 3050 ABS + Polyurethane

PHU9910 / 150370

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.