MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Wacker Silres® BS 66 Silicone Masonry Water Repellent
Categories: Polymer; Thermoset; Silicone

Material Notes: Product description: SILRES® BS 66 is a liquid oligomeric siloxane which is intended primarily for in-plant water-repellent treatment of aerated concrete. It may also be diluted with organic solvents for use as a water repellent for facades.

Application: Undiluted SILRES® BS 66 serves as a water-repellent admixture for aerated concrete. Even when added in very small quantities, it dramatically reduces water absorption, and also optimizes the concrete's pore structure. When used as a water repellent for facades, SILRES® BS 66 is diluted with organic solvents. The resulting solutions are characterized by their good depth of penetration and excellent resistance to alkalis. The product may be applied to practically all absorbent mineral substrates, such as bricks, sand-lime brick, concrete, natural stone, mineral paints and plasters. When the main focus is a pronounced beading effect, it is preferable to use the all-round water-repellent agent SILRES® BS 290.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.03 g/cc0.0372 lb/in³DIN 51757
Viscosity 12 - 17 cP12 - 17 cPdynamic
 
Thermal PropertiesMetricEnglishComments
Flash Point 50.0 °C122 °FISO 2719
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %"Clear" but manufacturer does not quantify.
 
Descriptive Properties
Active ingredients (%)100
Appearanceclear, colorless

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PWACK9540 / 205069

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.