MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
American Pau Marfim Wood
Categories: Wood and Natural Products; Wood; Hardwood

Material Notes: Dust may be irritant
Usual surface texture: Medium
Dimensional changes when dried lumber is subjected to variations in humidity during service: Large
Resistance to fungal decay (Heartwood in ground contact): Non-durable (5 to 10 years)
Common Applications: Interior and exterior joinery, furniture. Flooring

Key Words: Balfourodendron Riedelianum; Timber, Lumber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.730 g/ccGreen
Density 0.800 g/cc15% Moisture Content
 
Mechanical PropertiesOriginal ValueComments
Modulus of Rupture 0.0993 GPaStatic Bending, Green
 0.1303 GPaStatic Bending, 12% Moisture
Flexural Modulus 11400 MPaStatic Bending, Green
Compressive Strength 41.9 MPaParallel to Grain, Green
 56.5 MPaParallel to Grain, 12% Moisture
Machinability 100 %Good Relative to Other Wood
 
Thermal PropertiesOriginal ValueComments
Shrinkage 4.6 %Radial Shrinkage Green to Oven Dry
 8.8 %Tangential Shrinkage Green to Oven Dry
 13.4 %Volumetric Shrinkage Green to Oven Dry
 
Descriptive Properties
ColorYellowUsual for heartwood

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
A. Schulman POLYBATCHâ„¢ Ivory 90033/4 Concentrate Based In LDPE
American Black Walnut Wood
Silver Maple (Water Maple, White Maple), Soft Wood
American Andiroba Wood
American Black Ash (Brown Ash) Wood

PTSA730 / 71279

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.