MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polynt POLYCOR® M1 PA Gel Coat
Categories: Polymer; Thermoset

Material Notes: A pre-accelerated gel coat base on unsaturated polyester resin. It is cured using MEKP peroxide.

Appearance: Product is available in white, off-white and wide range of colors and can be color matched according to a particular demand. The product is formulated to assure a hide in wet film thickness of 500µm. However some bright shades may have a hide slightly lower opacity.

Properties / Advantages: The product is easy to use with highly controlled rheological properties providing high resistance to sagging.

Application: This gel coat is ready to use by application with airless spray equipment. Mix the product slowly but thoroughly for 10 minutes prior to each shift start up. Apply the correct film thickness. A wet film thickness between 300 to 600µm is required ideally in 3 even passes. Check that the correct level of MEKP is added. A level of 1,8% is recommended. Do not use more than 3% or lower than 1,2% MEKP catalyst. Minimum application temperature : 15°C This product is not designed for use with a roller or brush.

Use Areas: Product is recommended for the manufacture of industrial pieces requiring additional fire retardance. The product was designed for INTERNAL pieces ONLY.

Information provided by Polynt Composites.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.52 - 1.58 g/cc0.0549 - 0.0571 lb/in³
Solids Content 70 - 76 %70 - 76 %15mn at 150°C
Viscosity 16000 - 19000 cP16000 - 19000 cPSpindle 4 - 4 rpm
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 55.0 MPa7980 psiISO 527
Elongation at Break 2.2 %2.2 %ISO 527
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 57.0 °C135 °FNFT ISO 75
 
Processing PropertiesMetricEnglishComments
Cure Time  30.0 - 40.0 min
@Temperature 25.0 °C
0.500 - 0.667 hour
@Temperature 77.0 °F
Peak time; 200g - 25°C - 1,8% MEKP
 40.0 - 50.0 min
@Temperature 20.0 °C
0.667 - 0.833 hour
@Temperature 68.0 °F
Film cure; 500µ - 20°C - 2% MEKP
Gel Time 10.0 - 14.0 min
@Temperature 25.0 °C
10.0 - 14.0 min
@Temperature 77.0 °F
200g - 25°C - 1,8% MEKP
Shelf Life 4.00 Month4.00 Month
 
Descriptive Properties
Peak Exotherm110-140°C200g - 25°C - 1,8% MEKP
Sag Resistance500 µmwet
Thixotropic Index6.5-82/20 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPOLYN9247 / 231842

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.