MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Fluorseals PTFE 25% carbon filled
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); Polytetrafluoroethylene (PTFE), Carbon Fiber Filled

Material Notes: Improved compressive strength, wear resistance and thermal conductivity.

Information provided by TEKU GmbH Fluorkunststoffe, a distributor of Fluorseals materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.09 g/ccASTM 1457-62 T
Deformation 6.0 %14 MPa, 100 h, 23°C; ASTM D621-59
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 38.0 MPaASTM 1457-62 T
Tensile Strength at Break 14.0 MPaASTM 1457-62 T
Elongation at Break 170 %ASTM 1457-62 T
Coefficient of Friction, Dynamic 0.12 - 0.14v = 1 m/s
 0.12 - 0.15v = 1.9 m/s
Abrasion 0.55mm of depth after 200 hrs load duration; Partner Material ST 50
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1000 ohm-cmDIN 53482
Surface Resistance 1000 ohmDIN 53482
 
Thermal PropertiesOriginal ValueComments
CTE, linear 100 µm/m-°C
@Temperature 100 °C
DIN 52328
Thermal Conductivity 0.700 W/m-KDIN 52612

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M Dyneon™ CC191-HE PTFE, 25% Carbon/Graphite Filled
AGC Fluon® PB3060 60% Bronze, PTFE Filled Compound
Isoflon PTFE + 25% Carbon Polytetrafluoroethylene with 25% Carbon
AGC Fluon® PB2510 10% Carbon Fiber, PTFE Filled Compound
AGC Fluon® FC160-60 PTFE, 60% Bronze Filled

PTEKU3 / 70056

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.