MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Tra-Con Tra-Bond 2113 Clear Low Viscosity Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy

Material Notes: TRA-BOND 2113 is a clear, low viscosity epoxy adhesive system that contains no solvents, cures at room temperature, has excellent flowability and wetting characteristics, and adheres strongly to glass, ceramics, most metals and many plastics. It is particularly recommended for assembly and repair work of fiber optic and other high performance electronic and aerospace systems and components, and for structural laminating applications where an initial low viscosity and near transparent "color" are needed. Fully cured TRA-BOND 2113 is a good electrical insulator, provides excellent resistance to weather, galvanic action, salt solutions and many other chemicals including mild acid and alkalis, petroleum solvents, lubricating oils, jet fuels and gasoline, and alcohol.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.16 g/ccMixed
Viscosity 300 cP
@Temperature 25.0 °C
After mixing
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 88
Adhesive Bond Strength 2200 psiLap shear, alum to alum, 2 hrs @ 65°C
Izod Impact, Notched 0.240 ft-lb/in
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 6.00e+13 ohm-cm
 1.00e+10 ohm-cm
@Temperature 100 °C
Dielectric Constant 4.3
@Frequency 1000 Hz
Dielectric Strength 410 V/mil
Dissipation Factor 0.020
@Frequency 1000 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 60.0 µm/m-°C
@Temperature 20.0 °C
Maximum Service Temperature, Air 130 °C
Minimum Service Temperature, Air -60.0 °C
Glass Transition Temp, Tg 77.0 °CUltimate Tg
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %clear; thickness not quantified
 
Processing PropertiesOriginal ValueComments
Cure Time 4.00 hour
@Temperature 65.0 °C
 24.0 hour
@Temperature 25.0 °C
Pot Life 30 min
 
Descriptive Properties
Color Transparent, Clear
Mix Ratio, parts by weight100/11Resin/Hardener
Thixotropic Index 1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Tra-Con Tra-Bond 526M05 Rapid Low Temperature Cure Adhesive

PTRAC014 / 70942

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.