Product Description: LD 124.MS blown film resin offers an excellent balance of optical and strength properties for general purpose clear film applications. Availability: Latin America, North America and South America Additive: - Antiblock: 2000 ppm
- Slip: 400 ppm
- Thermal Stabilizer: Yes
Applications: - Blend Partner
- Food Packaging
- Form Fill and Seal Packaging
- High Clarity Film
- Lamination Film
- Light Duty Shrink Film
- Mail Bag
- Produce Bags
- Textile Packaging
Information provided by ExxonMobil |