MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ecomass® 1950TU76 Tungsten Filled Polyamide
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 610 (PA610)

Material Notes: Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applications
  • Tungsten Powder Filled Polyamide (PA6/10)
  • Very Good Toughness

Information provided by Technical Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 3.80 g/ccASTM D792
Linear Mold Shrinkage 0.010 - 0.012 cm/cmInternal
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 43.0 MPaISO 527
Elongation at Break 10.5 %ISO 527
Tensile Modulus 2.968 GPaISO 527
Flexural Modulus 2.40 GPaISO 178
Izod Impact, Notched (ISO) 6.30 kJ/m²ISO 180-A
 
Processing PropertiesOriginal ValueComments
Melt Temperature 230 - 250 °C
Mold Temperature 65.0 - 80.0 °C
Drying Temperature 80.0 °C
Dry Time 4 - 6 hour
Moisture Content <= 0.20 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ecomass® 3608TU96 Tungsten Filled Polyethylene
Ecomass® 3620BX60 18% Borated Polyethylene (HDPE)

PECOM47 / 35457

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.