MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Elkem (Bluestar Silicones) CAF® 99 AXAD BLACK Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: Description: CAF 99 AXAD BLACK is a two component room temperature vulcanising silicone elastomer.
  • activated acetic,
  • thixiotropic,
  • black.
Applications: CAF 99 AXAD BLACK is mainly used in sealing and bonding applications for :
  • Household electrical appliances: oven fascias, oven door staples, oven door windows, vitroceramic hobs.
  • Glass bonding applications: bonding of boat port-hole glass, cockpit windows.
Advantages: CAF 99 AXAD BLACK cures quickly at room temperature without release of acetic acid and its setting time can be accelerated with temperature. CAF 99 AXAD BLACK sets in confined spaces and in high section thicknesses. CAF 99 AXAD BLACK gives very high mechanical performance levels, very good heat stability, primerless adhesion on many surfaces and good resistance to chemical agents. CAF 99 AXAD BLACK therefore provides perfect assembly and complete sealing when jointing different materials subject to thermal strains.

Information provided by Bluestar Silicones

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.11 g/ccPart A; ISO R1183
 1.15 g/ccafter curing; ASTM D297
 1.43 g/ccPart B; ISO R1183
Storage Temperature 2.00 - 30.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 51ASTM D2240
 25
@Temperature 23.0 °C,
Time 3600 sec
 38
@Temperature 23.0 °C,
Time 7200 sec
 41
@Temperature 23.0 °C,
Time 14400 sec
 38
@Treatment Temp. 100 °C,
Time 3600 sec
 42
@Treatment Temp. 150 °C,
Time 3600 sec
 42
@Treatment Temp. 100 °C,
Time 7200 sec
 45
@Treatment Temp. 150 °C,
Time 7200 sec
 45
@Treatment Temp. 100 °C,
Time 14400 sec
 47
@Treatment Temp. 150 °C,
Time 14400 sec
Tensile Strength 276 psiadhesion on AG 3 aluminum, cure 1 day at RT, 80% cohesive failure
 334 psiadhesion on AG 3 aluminum, cure 3 day at RT, 100% cohesive failure
 363 psiadhesion on AG 3 aluminum, cure 7 day at RT, 100% cohesive failure
 363 psiadhesion on AG 3 aluminum, cure 7 day at RT+3 days at 250°C+1 day at RT, 100% cohesive failure
 624 psiASTM D412
Elongation at Break 235 %ASTM D412
100% Modulus 0.334 ksi
@Strain 100 %
ASTM D412
Tear Strength 57.1 pliASTM D624
Compression Set 35 %
@Time 259000 sec
cured for 7 days, 125°C temp on specimen compressed by 25% for 3 days
 45 %
@Time 259000 sec
cured for 7 days, 150°C temp on specimen compressed by 25% for 3 days
 50 %
@Time 259000 sec
cured for 1 day, 125°C temp on specimen compressed by 25% for 3 days
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 2.00e+15 ohm-cmASTM D257
Dielectric Constant 3.2
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 457 V/milASTM D419
Dissipation Factor 0.0040
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.220 W/m-K
@Temperature 150 °C
Standard NF x 10021
 0.250 W/m-K
@Temperature 25.0 °C
Standard NF x 10021
Maximum Service Temperature, Air 250 °C
@Time 3.60e+6 sec
 300 °C
@Time 259000 sec
Peak
Brittleness Temperature -70.0 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life 18.0 Month
 
Descriptive Properties
AppearancePart A
 Part B
ColorBlackPart A
 BlackPart B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Elkem (Bluestar Silicones) CAF® 1 Extra Fluid Silicone Rubber
Elkem (Bluestar Silicones) CAF® 7037 Silicone Rubber
Rogers Arlon 51073R031 0.0311" (0.79 mm) Cured Silicone Rubber with Fiberglass Substrate
Elkem (Bluestar Silicones) BLUESIL™ VRM-65 Hi-Pro Green Silicone Rubber
Elkem (Bluestar Silicones) Bluesil™ TCS 7537 A/B Silicone Polyaddition for Technical Textiles

PBLUST092 / 191068

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.