MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
PoolKemie RESINPOL E 386 Polyester resin
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Description: Unsaturated orthophalic acid based polyester resin dissolved in styrene and pre-accelerated. This resin combines good mechanical characteristics and low shrinkage with excellent moistening of reinforcement fibers and mineral fillers.

Application: The E 386 resin is recommended for the construction of bodywork, sanitary items, helmets, industrial machine parts, and other items that require good mechanical characteristics. Due to its rheological features, it is mainly used for the manual forming of flat items, for press moulding at low to medium temperatures, for the casting of ornamental or sanitary items, or for the production of synthetic marble and agglomerate marble.

Information provided by Poolkemie

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.00 - 1.20 g/ccPK03
Solids Content 62 - 66 %PK04
Viscosity 350 - 400 cPA+B
Brookfield Viscosity 400 - 500 cP(19.6 sec-1) PK01
Storage Temperature <= 20.0 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 55.0 - 65.0 MPa
Elongation at Break 2.0 - 2.4 %
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 68.0 - 76.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 14.0 - 22.0 min
Pot Life 6.00 - 10.0 min
Gel Time 5.50 - 7.50 minPK02
Shelf Life 6.00 Month
 
Descriptive Properties
ColorAmber Transparent
Exothermic peak14-18 mintime, PK02
 160-170°CTemperature, PK02
Mixing ratio100:2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPOOLK057 / 318536

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.