MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
C.O.I.M. DIEXTER® G217 Polyol Polyester
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoplastic; Polyester, TP

Material Notes: Description: The DIEXTER® line of products offers a vast selection of polyol polyesters with different molecular weights and functions. DIEXTER® is sold for the production of polyurethanes in virtually every field of application. These saturated polyester resins can be used in applications ranging from the production of slab stocks to synthetic leathers and thermoplastics. Basic Composition = DEG
Information provided by P.A.T. Products, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 3600 - 4400 cP
@Temperature 35.0 °C
Molecular Weight 2000 g/mol
 
Descriptive Properties
Hydroxyl Number (mg KOH/gr)54Min
 58Max
Structurelinear

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
C.O.I.M. DIEXTER® G172 Polyol Polyester
C.O.I.M. DIEXTER® G215 Polyol Polyester
C.O.I.M. DIEXTER® G222 Polyol Polyester
C.O.I.M. DIEXTER® G224 Polyol Polyester
C.O.I.M. DIEXTER® G174 Polyol Polyester

PCOIM055 / 28658

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.