MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Eastman AdapT® 203 MDEA-based solvent
Categories: Fluid; Solvent

Material Notes: CAS No. 105-59 -9

Product Description: AdapT 203 is a formulated MDEA-based solvent designed for the deep removal of CO2 from CO2 containing gas streams. The removal of sour or acid gas components such as hydrogen sulfide (H2S) or carbon dioxide (CO2) from gas streams is a common process, known as acid gas removal or gas sweetening. These impurities have to be eliminated or reduced to a specified level, for a variety of reasons: toxicity (H2S), corrosiveness of the gas, low caloric value, environment or other reasons depending on the application of the gas. For over 50 years, alkanolamines have been used for acid gas treatment in natural gas and petroleum processing industries. AdapT solvent range is based on today’s most advanced and preferred alkanolamine for gas treatment technology: MDEA, and MDEA-based formulations.

Application/Uses:

  • Acid gas removal
Key Attributes:
  • Degradation resistance
  • High solvent loading
  • Low capex and opex
  • Low corrosiveness
  • Low energy requirements
  • Low solvent make-up

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.04 g/cc0.0376 lb/in³
Viscosity 200 cP200 cP
Vapor Pressure <= 0.00132 bar<= 0.988 torr
 
Thermal PropertiesMetricEnglishComments
Melting Point -20.0 °C-4.00 °FFreezing Point
Flash Point >= 120 °C>= 248 °FClosed Cup
 
Descriptive Properties
AppearanceColorless to light yellow liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEATM5008 / 222202

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.