MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Trinseo MAGNUM™ 8391 Acrylonitrile Butadiene Styrene (ABS) Resin
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: MAGNUM™ 8391 ABS combines an excellent gloss appearance with high flow and medium impact performance. The mass (continuous process) ABS technology ensures an ABS resin that combines excellent processability with a stable light base color that is ideal for self-coloring.

Applications:

  • Household Appliance
  • Consumer Goods
  • Toys

Information provided by Trinseo.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.05 g/ccASTM D792
Apparent Bulk Density 0.650 g/ccISO 60
Linear Mold Shrinkage, Flow 0.0040 - 0.0070 in/inISO 294-4
Melt Flow 8.0 g/10 min
@Load 3.80 kg,
Temperature 230 °C
ASTM D1238
 28 g/10 min
@Load 10.0 kg,
Temperature 220 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 108ASTM D785
Tensile Strength at Break 35.0 MPaInjection Molded, 50 mm/min; ASTM D638
Tensile Strength, Yield 48.0 MPaInjection Molded, 50 mm/min; ASTM D638
 45.0 MPa
@Thickness 3.20 mm
Injection Molded; ISO 527-2/50
 47.0 MPa
@Thickness 3.20 mm
Injection Molded; ISO 527-2/100
Tensile Modulus 2340 MPa
@Thickness 3.20 mm
Injection Molded; ISO 527-2
Flexural Strength 75.0 MPa1.3 mm/min; ASTM D790
 70.0 MPa
@Thickness 3.20 mm
Injection Molded, 2.0 mm/min, 3-points; ISO 178
Flexural Modulus 2400 MPaInjection Molded, 2.0 mm/min, 3-points; ISO 178
 2480 MPa1.3 mm/min; ASTM D790
Izod Impact, Notched 230 J/mASTM D256
Izod Impact, Notched (ISO) 9.00 kJ/m²
@Temperature -30.0 °C
Injection Molded; ISO 180/A
 19.0 kJ/m²
@Temperature 23.0 °C
Injection Molded; ISO 180/A
Charpy Impact, Notched 9.00 kJ/m²
@Temperature -30.0 °C
Injection Molded; ISO 179/1eA
 19.0 kJ/m²
@Temperature 23.0 °C
Injection Molded; ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 87.0 °CUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 74.0 °CUnannealed; ASTM D648
 95.0 °CAnnealed; ISO 75-2/A
Vicat Softening Point 95.0 °CISO 306/B50
 99.0 °CASTM D1525
Flammability, UL94 HB
@Thickness 1.50 mm
 HB
@Thickness 3.00 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Trinseo Magnum™ 3453 Acrylonitrile Butadiene Styrene (ABS)
Trinseo Magnum™ 8391 MED Acrylonitrile Butadiene Styrene (ABS) Resin
Chi Mei Polylac® PA-709 ABS
Lotte Advanced Materials Starex® SD-0150W ABS, Unreinforced
INEOS Styrolution Terluran® GP-22 ABS

PDWST071 / 142280

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.