MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Techmer ES Plastiblend® PC/PET IM 1016 UV
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/PET Polyester Blend; Polyester, TP; Polyethylene Terephthalate (PET)

Material Notes: Availability: North America

Forms: Pellets

Additive: Impact Modifier and UV Stabilizer

Features: Impact Modified

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.22 g/ccASTM D792
Water Absorption 0.17 %
@Time 86400 sec
ASTM D570
Melt Flow 12 g/10 min
@Load 5.00 kg,
Temperature 265 °C
ASTM D1238
 28 g/10 min
@Load 2.16 kg,
Temperature 285 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 117ASTM D785
Tensile Strength, Yield 7800 psiASTM D638
Elongation at Break 120 %ASTM D638
Flexural Yield Strength 13000 psiASTM D790
Flexural Modulus 310000 psiASTM D790
Izod Impact, Notched 12.0 ft-lb/in
@Thickness 3.17 mm,
Temperature -40.0 °C
ASTM D256
 16.0 ft-lb/in
@Thickness 3.17 mm,
Temperature 22.8 °C
ASTM D256
Dart Drop, Total Energy 3.79 ft-lb
@Temperature -40.0 °C
ASTM D3763
 3.92 ft-lb
@Temperature 22.8 °C
ASTM D3763
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 7.00e+15 ohm-cmASTM D257
Dielectric Strength 700 V/milMethod A (Short-Time); ASTM D149
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 35.0 µin/in-°FASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 240 °FUnannealed; ASTM D648
Flammability, UL94 HB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
A. Schulman Diamond DIAMALOY 223U UV Stabilized, PC/PET Alloy
RTP Company RTP 1102 UV  Polyethylene Terephthalate (PET) Glass Fiber 15% - UV Stable
Lotte Advanced Materials Infino® AE-2130 PC/PET, 5% MF
ABW Polymers PC/PET Alloy
A. Schulman Lucent PC/PET-1515 Polycarbonate+PET, General Purpose, Injection Grade

PTPC1233 / 137171

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.