MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics Custom PZT 701 Piezo Ceramic  (discontinued **)
Categories: Ceramic; Piezoelectric

Material Notes:

Information provided by Morgan Advanced Materials. Morgan's electroceramic business was sold to Ceramtec in 2018.

Key Words: PZT 701
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.80 g/cc
 
Mechanical PropertiesOriginal ValueComments
Poissons Ratio 0.31
 
Electrical PropertiesOriginal ValueComments
Curie Temperature 350 °C
Dielectric Strength 1.28 kV/mm
Dissipation Factor 1.38tan d
Piezoelectric Longitudinal Coupling Factor, k33 0.67
Piezoelectric Transverse Voltage Coefficient, d31, 10^-12 m/V 59
Piezoelectric Shear Charge Coefficient, d15, 10^-12 m/V 360
Piezoelectric Longitudinal Voltage Coefficient, g33, 10^-3 V-m/N 45.6
Piezoelectric Planar Coupling Factor, kp 0.51
Piezoelectric Mechanical Q 570
Piezoelectric Shear Coupling Factor, k15 0.68
Piezoelectric Longitudinal Charge Coefficient, d33, 10^-12 m/V 166
Piezoelectric Transverse Voltage Coefficient, g31, 10^-3 V-m/N 16.2
Piezoelectric Shear Voltage Coefficient, g15, 10^-3 V-m/N 50
Piezoelectric Transverse Coupling Factor, k31 0.30
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 175 °C
 
Descriptive Properties
Piezoelectric PropertiesCoupling factor (kt)
 Hz-m Frequency Constant (N1)
 Hz-m Frequency Constant (N3t)
 Hz-m Frequency Constant (N5)
 Hz-m Frequency Constant (Np)
Time StabilityAging Rate (d constant): 0.1 % per decade
 Aging Rate (dielectric):0.2 % per decade
 Aging Rate (frequency): 0.0 % per decade
 Aging Rate( coupling): -0.1 % per decade

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Morgan Advanced Ceramics Custom PZT 601 Piezo Ceramic
Morgan Advanced Ceramics PZT800 Series PZT 806 Piezo Ceramic
Channel Industries 5804 Lead Zirconate Titanate Piezoelectric
Channel Industries 5800 Lead Zirconate Titanate Piezoelectric
Harris Acoustic Sensors EC-65 Lead Zirconium Titanate Piezoelectric

CMORF5031 / 200269

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.