MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Outokumpu 4307 Cr-Ni Austenitic Stainless Steel
Categories: Metal; Ferrous Metal; Austenitic; Stainless Steel

Material Notes: General purpose steel with good corrosion resistance.

Applications: Wide variety of applications in construction, chemical, petroleum, automobile, and domestic appliance markets.

Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms.

Key Words: EN 1.4307; ASTM 304L; JIS SUS 304L
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.90 g/ccRT
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 165Outokumpu Typical, 20°C, Hot rolled plate (Quarto); EN 10003-1
 175Outokumpu Typical, 20°C, Cold rolled strip/sheet; EN 10003-1
Tensile Strength, Ultimate >= 500 MPaEN 10002-1
 580 MPaOutokumpu Typical, Hot Rolled Plate (Quarto); EN 10002-1
 340 MPa
@Temperature 300 °C
EN min.; EN 10002-5
 360 MPa
@Temperature 200 °C
EN min.; EN 10002-5
 410 MPa
@Temperature 100 °C
EN min.; EN 10002-5
 830 MPa
@Temperature -80.0 °C
EN min; EN 10002-5
 1200 MPa
@Temperature -196 °C
EN min; EN 10002-5
Tensile Strength, Yield 200 MPa
@Strain 0.2 %
EN min., RT; EN 10002-1
 240 MPa
@Strain 1 %
EN min., RT; EN 10002-1
 280 MPa
@Strain 0.2 %
Outokumpu Typical, Hot Rolled Plate (Quarto); EN 10002-1
 320 MPa
@Strain 1 %
Outokumpu Typical, Hot Rolled Plate (Quarto); EN 10002-1
 81.0 MPa
@Strain 0.2 %,
Temperature 500 °C
EN min.; EN 10002-5
 89.0 MPa
@Strain 0.2 %,
Temperature 400 °C
EN min.; EN 10002-5
 100 MPa
@Strain 0.2 %,
Temperature 300 °C
EN min.; EN 10002-5
 109 MPa
@Strain 1 %,
Temperature 500 °C
EN min.; EN 10002-5
 116 MPa
@Strain 1 %,
Temperature 400 °C
EN min.; EN 10002-5
 118 MPa
@Strain 0.2 %,
Temperature 200 °C
EN min.; EN 10002-5
 127 MPa
@Strain 1 %,
Temperature 300 °C
EN min.; EN 10002-5
 147 MPa
@Strain 0.2 %,
Temperature 100 °C
EN min.; EN 10002-5
 147 MPa
@Strain 1 %,
Temperature 200 °C
EN min.; EN 10002-5
 181 MPa
@Strain 1 %,
Temperature 100 °C
EN min.; EN 10002-5
 220 MPa
@Strain 0.2 %,
Temperature -80.0 °C
EN min.; EN 10002-5
 290 MPa
@Strain 1 %,
Temperature -80.0 °C
EN min.; EN 10002-5
 300 MPa
@Strain 0.2 %,
Temperature -196 °C
EN min.; EN 10002-5
 400 MPa
@Strain 1 %,
Temperature -196 °C
EN min.; EN 10002-5
Elongation at Break >= 45 %EN 10002-1
 55 %Outokumpu Typical, Hot Rolled Plate (Quarto); EN 10002-1
 30 %
@Temperature -196 °C
EN min
 35 %
@Temperature -80.0 °C
EN min
Modulus of Elasticity 200 GPaRT
 165 GPa
@Temperature 500 °C
 172 GPa
@Temperature 400 °C
 179 GPa
@Temperature 300 °C
 186 GPa
@Temperature 200 °C
 194 GPa
@Temperature 100 °C
Poissons Ratio 0.30RT
Shear Modulus 77.0 GPacalculated
Impact Test >= 60.0 JHot rolled plate/Cold rolled strip/sheet, 10x10mm test pieces; EN 10045-1
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000730 ohm-cmRT
 
Thermal PropertiesOriginal ValueComments
CTE, linear 16.0 µm/m-°C
@Temperature 100 °C
 18.0 µm/m-°C
@Temperature 400 °C
Specific Heat Capacity 0.500 J/g-°CRT
Thermal Conductivity 15.0 W/m-KRT
 20.0 W/m-K
@Temperature 400 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.020 %
Chromium, Cr 18.1 %
Iron, Fe 73.58 %
Nickel, Ni 8.3 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Schmolz + Bickenbach UGIMA 304/304L® Stainless Steel Bar
Industeel CLC 18.9 L General Purpose 18Cr-9Ni Austenitic Stainless Steel
Outokumpu 4404 Cr-Ni-Mo Austenitic Stainless Steel
Outokumpu 4571 Cr-Ni-Mo Austenitic Stainless Steel
Outokumpu 4845 High Temperature Austenitic Stainless Steel

NOUTOK13 / 18728

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.