MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC LNP™ THERMOCOMP™ Compound D351RC Polycarbonate (PC)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LNP THERMOCOMP D351RC compound is based on recycled Polycarbonate (PC) resin containing 30% glass fiber. Added features of this grade include: High Modulus, Low Warpage, Good Ductility, Non-Brominated & Non-Chlorinated Flame Retardant. Post-Consumer Recycling (PCR) Polycarbonate content up to 35%.

Features: Post-Consumer Recycled (PCR) content,High Stiffness,Enhanced Ductility,Flame Retardant,Non-Chlorinated,Non-Brominated,Low Warpage,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.425 g/ccASTM D792
Moisture Absorption 0.0200 %Injection Molding
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm24hrs; ASTM D955
Linear Mold Shrinkage, Transverse 0.0010 - 0.0030 cm/cm24hrs; ASTM D955
Melt Flow 27.3 g/10 min
@Load 2.16 kg,
Temperature 300 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 129 MPa5 mm/min; ASTM D638
Elongation at Break 2.2 %5 mm/min; ASTM D638
Tensile Modulus 9415 MPa5 mm/min; ASTM D638
Flexural Strength 180 MPabrk, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 8390 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 128 JASTM D256
Izod Impact, Unnotched 537 J/mASTM D4812
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 19.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
CTE, linear, Transverse to Flow 69.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
Deflection Temperature at 1.8 MPa (264 psi) 119 °C
@Thickness 3.20 mm
unannealed; ASTM D648
UL RTI, Electrical 80.0 °CUL 746B
UL RTI, Mechanical with Impact 80.0 °CUL 746B
UL RTI, Mechanical without Impact 80.0 °CUL 746B
Flammability, UL94 V-0
@Thickness >=0.800 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 285 - 305 °C
Zone 2 270 - 290 °C
Zone 3 280 - 300 °C
Melt Temperature 285 - 310 °CInjection Molding
Mold Temperature 80.0 - 110 °C
Drying Temperature 110 °CInjection Molding
Dry Time 3.00 - 6.00 hourInjection Molding
Back Pressure 0.100 - 0.300 MPa
Screw Speed 50 - 90 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH81486 / 289433

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.