Medium viscosity for good wet out of all synthetic composite fabrics and core materials. Slow cure speed hardener provides 4.5 to 6 hours of working time at 72°F (22°C). Elevated temperature cure is required; thermal and mechanical properties suitable for composite components and high temperature tooling and molds. Tg as high as 197°F (92°C) with proper post cure providing excellent temperature stability and great part cosmetics. Cost effective, high performance epoxy formulation for synthetic composite manufacturing. Quality-control tinting is available at no extra charge; simply add "QC" after the product code on your order.Information provided by Gougeon Brothers, Inc. |