MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Teknor Apex Telcar® TL-1522H Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping

Forms: Pellets

Processing Method: Extrusion; Injection Molding

Injection Notes: Injection Rate: Moderate-Fast

Extrusion Notes: Screw Speed: 30 to 100 rpm

Information Provided by Teknor Apex

Key Words: TPE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.18 g/cc1.18 g/ccASTM D792
Linear Mold Shrinkage 0.012 cm/cm0.012 in/inASTM D955
Linear Mold Shrinkage, Transverse 0.013 cm/cm0.013 in/inASTM D955
Melt Flow  17 g/10 min
@Load 2.16 kg,
Temperature 190 °C
17 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 57 g/10 min
@Load 2.16 kg,
Temperature 230 °C
57 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7070ASTM D2240
Tensile Strength at Break 5.24 MPa760 psiASTM D412
Tensile Stress at Strain  1.86 MPa
@Strain 100 %
270 psi
@Strain 100 %
ASTM D412
 2.83 MPa
@Strain 300 %
410 psi
@Strain 300 %
ASTM D412
Elongation at Break 650 %650 %ASTM D412
Tear Strength 24.5 kN/m140 pliDie C; ASTM D624
Compression Set  30 %
@Temperature 22.8 °C,
Time 79200 sec
30 %
@Temperature 73.0 °F,
Time 22.0 hour
ASTM D395B
 82 %
@Temperature 70.0 °C,
Time 79200 sec
82 %
@Temperature 158 °F,
Time 22.0 hour
ASTM D395B
 98 %
@Temperature 100 °C,
Time 79200 sec
98 %
@Temperature 212 °F,
Time 22.0 hour
ASTM D395B
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity  1.60e+16 ohm-cm
@Temperature 50.0 °C
1.60e+16 ohm-cm
@Temperature 122 °F
ASTM D257
 7.40e+18 ohm-cm
@Temperature 22.8 °C
7.40e+18 ohm-cm
@Temperature 73.0 °F
ASTM D257
Dielectric Strength 39.4 kV/mm1000 kV/inASTM D419
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 171 - 193 °C340 - 380 °F
Middle Barrel Temperature 177 - 199 °C350 - 390 °F
Front Barrel Temperature 182 - 204 °C360 - 400 °F
Nozzle Temperature 188 - 210 °C370 - 410 °F
Zone 1 166 - 188 °C330 - 370 °F
Zone 2 171 - 193 °C340 - 380 °F
Zone 3 177 - 199 °C350 - 390 °F
Zone 5 182 - 204 °C360 - 400 °F
Die Temperature 190 - 210 °C374 - 410 °F
Melt Temperature 188 - 210 °C370 - 410 °FProcessing Temperature
Mold Temperature 25.0 - 65.6 °C77.0 - 150 °F
Injection Pressure 1.38 - 6.89 MPa200 - 1000 psi
Back Pressure 0.172 - 0.345 MPa25.0 - 50.0 psi
Cushion 0.381 - 2.54 cm0.150 - 1.00 in
Screw Speed 50 - 100 rpm50 - 100 rpm
 
Descriptive Properties
AppearanceOpaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTEKNP405 / 129486

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.