MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

AISI Type S24000 Stainless Steel, sheet, 30% cold reduction
Categories: Metal; Ferrous Metal; Heat Resisting; Stainless Steel

Material Notes: Low nickel, austenitic with good stress corrosion resistance and low magnetic permeability, usually not subject to intergranular attack. Typical applications include heat exchangers, process vessels, pipe and tubing, riser pipe for underground power transmission, and cryogenic tanks, valves and piping.

Key Words: UNS S24000, ASME SA240 (XM-29), ASME SA249 (XM-29), ASME SA312 (XM-29), ASME SA688 (XM-29), ASTM A240 (XM-29), ASTM A249 (XM-29), ASTM A269 (XM-29), ASTM A276 (XM-29), ASTM A312 (XM-29), ASTM A313 (XM-29), ASTM A358 (XM-29), ASTM A412 (XM-29), ASTM A479 (XM-29), ASTM A580 (XM-29), ASTM A688 (XM-29), T S24000
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.75 g/cc0.280 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 379379Converted from Rockwell C hardness.
Hardness, Knoop 414414Converted from Rockwell C hardness.
Hardness, Rockwell C 4141
Hardness, Vickers 399399Converted from Rockwell C hardness.
Tensile Strength, Ultimate 1270 MPa184000 psi
Tensile Strength, Yield 1150 MPa
@Strain 0.2 %
167000 psi
@Strain 0.2 %
Elongation at Break 10 %10 %in 50 mm
Modulus of Elasticity 200 GPa29000 ksiTypical for stainless steel
Machinability 30 %30 %Based on 100% machinability for AISI 1212 steel.
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity  0.0000740 ohm-cm
@Temperature 25.0 °C
0.0000740 ohm-cm
@Temperature 77.0 °F
 0.0000800 ohm-cm
@Temperature 100 °C
0.0000800 ohm-cm
@Temperature 212 °F
 0.0000870 ohm-cm
@Temperature 200 °C
0.0000870 ohm-cm
@Temperature 392 °F
 0.000100 ohm-cm
@Temperature 400 °C
0.000100 ohm-cm
@Temperature 752 °F
 0.000111 ohm-cm
@Temperature 600 °C
0.000111 ohm-cm
@Temperature 1110 °F
 0.000119 ohm-cm
@Temperature 800 °C
0.000119 ohm-cm
@Temperature 1470 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear  16.0 µm/m-°C
@Temperature 25.0 - 93.0 °C
8.89 µin/in-°F
@Temperature 77.0 - 199 °F
 16.6 µm/m-°C
@Temperature 24.0 - 205 °C
9.22 µin/in-°F
@Temperature 75.2 - 401 °F
 17.5 µm/m-°C
@Temperature 25.0 - 315 °C
9.72 µin/in-°F
@Temperature 77.0 - 599 °F
 18.2 µm/m-°C
@Temperature 25.0 - 425 °C
10.1 µin/in-°F
@Temperature 77.0 - 797 °F
 18.7 µm/m-°C
@Temperature 25.0 - 540 °C
10.4 µin/in-°F
@Temperature 77.0 - 1000 °F
 19.4 µm/m-°C
@Temperature 25.0 - 650 °C
10.8 µin/in-°F
@Temperature 77.0 - 1200 °F
 20.2 µm/m-°C
@Temperature 25.0 - 760 °C
11.2 µin/in-°F
@Temperature 77.0 - 1400 °F
 20.5 µm/m-°C
@Temperature 25.0 - 870 °C
11.4 µin/in-°F
@Temperature 77.0 - 1600 °F
 20.5 µm/m-°C
@Temperature 25.0 - 980 °C
11.4 µin/in-°F
@Temperature 77.0 - 1800 °F
Specific Heat Capacity 0.480 J/g-°C0.115 BTU/lb-°FTypical value for stainless steel.
Thermal Conductivity  15.9 W/m-K
@Temperature 100 °C
110 BTU-in/hr-ft²-°F
@Temperature 212 °F
 17.3 W/m-K
@Temperature 200 °C
120 BTU-in/hr-ft²-°F
@Temperature 392 °F
 18.9 W/m-K
@Temperature 300 °C
131 BTU-in/hr-ft²-°F
@Temperature 572 °F
 20.4 W/m-K
@Temperature 400 °C
142 BTU-in/hr-ft²-°F
@Temperature 752 °F
 22.0 W/m-K
@Temperature 500 °C
153 BTU-in/hr-ft²-°F
@Temperature 932 °F
 23.4 W/m-K
@Temperature 600 °C
162 BTU-in/hr-ft²-°F
@Temperature 1110 °F
 24.7 W/m-K
@Temperature 700 °C
171 BTU-in/hr-ft²-°F
@Temperature 1290 °F
 26.1 W/m-K
@Temperature 800 °C
181 BTU-in/hr-ft²-°F
@Temperature 1470 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.080 %<= 0.080 %
Chromium, Cr 18 %18 %
Iron, Fe 64 %64 %
Manganese, Mn 13 %13 %
Nickel, Ni 3.13 %3.13 %
Nitrogen, N 0.30 %0.30 %
Phosphorus, P <= 0.060 %<= 0.060 %
Silicon, Si <= 1.0 %<= 1.0 %
Sulfur, S <= 0.030 %<= 0.030 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI 1006 Steel, cold drawn
308 Stainless steel, cold drawn wire, full hardened
AISI 1015 Steel, normalized at 925°C (1700°F), 50 mm (2 in.) round
AISI 1060 Steel, oil quenched 845°C (1550°F), 480°C (900°F) temper, 13 mm (0.5 in.) round
AISI 1022 Steel, heat treated, reheated to 830°C (1525°F), 25 mm (1 in.) round

MQM240Q / 13782

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.