MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Eastman Tenite Propionate 350E0096914 Natural, Trsp Cellulose Acetate Propionate
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Cellulosic; Cellulose Acetate Propionate, Molded

Material Notes: Product Description: Tenite™ cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite™ cellulosic plastics differ with plasticizer levels. Lower plasticizer content yields a harder surface, higher heat resistance, greater rigidity, higher tensile strength, and better dimensional stability. Higher plasticizer content increases impact strength. Tenite™ cellulosic plastics are available in natural, clear, selected ambers or smoke transparents and black translucent. Color concentrates are available in let-down ratios from 10:1 to 40:1. Tenite™ Cellulose Acetate Propionate 350-14 has a plasticizer level of 14%. It meets FDA requirements for certain food-contact applications when supplied in specific FDA color numbers.

Applications/Uses:

  • Medical

Key Words: CAP
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccASTM D792
Water Absorption 1.6 %24 hour immersion; ASTM D570
Linear Mold Shrinkage 0.0020 - 0.0060 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 80ASTM D785
Tensile Strength, Ultimate 36.5 MPaASTM D638
Tensile Strength, Yield 31.7 MPaASTM D638
Elongation at Break 40 %ASTM D638
Flexural Yield Strength 41.4 MPaASTM D790
Flexural Modulus 1.517 GPaASTM D790
Izod Impact, Notched 4.16 J/cmASTM D256
 1.07 J/cm
@Temperature -40.0 °C
ASTM D256
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+13 - 1.00e+15 ohm-cmASTM D257
Dielectric Constant 3.3 - 3.8
@Frequency 1e+6 Hz
ASTM D 150
Dielectric Strength 11.8 - 18.7 kV/mmASTM D149
Dissipation Factor 0.010 - 0.15
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 11.0 - 17.0 µm/m-°C
@Temperature 20.0 °C
ASTM D696
Specific Heat Capacity 1.26 - 1.67 J/g-°CDSC
Thermal Conductivity 0.170 - 0.330 W/m-KASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 88.0 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °CConditioned 4 hours @ 70°C (158°F); ASTM D648
Vicat Softening Point 105 °CConditioned 4 hours @ 70°C (158°F); ASTM D1525
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.46 - 1.49ASTM D542
Haze <= 8.5 %
@Thickness 1.52 mm
ASTM D1003
Transmission, Visible >= 90 %
@Thickness 1.52 mm
ASTM E308

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Eastman Tenite Propionate 360E0096916 Natural, Trsp Cellulose Acetate Propionate
Eastman Tenite Propionate 307A2R30013 Natural, Trsp Cellulose Acetate Propionate
Eastman Tenite Propionate 380A4000010 Clear, Trsp Cellulose Acetate Propionate
Eastman Tenite Butyrate 576E3720010 Clear, Trsp Cellulose Acetate Butyrate
Eastman Tenite Butyrate 575E3720010 Clear, Trsp Cellulose Acetate Butyrate

PEA245 / 35263

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.