MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Ensinger Tecanat™ GF20 20% Glass Reinforced Polycarbonate (PC)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, 20% Glass Filled

Material Notes: Tenacat™ GF20 is typically used in business equipment where gears, rollers, interlam mechanical parts, connectors and relays are required. The automotive industry uses polycarbonate materials for pumps, valves, light bezels and instrument panels.
  • Excellent dimensional stability
  • Transparency
  • Good machinability

    Information Provided by Ensinger Inc.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.34 g/cc
Water Absorption 0.16 %at 24 hours; ASTM D570
Water Absorption at Saturation 0.29 %ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 16000 psiASTM D638
Elongation at Break 5.0 %ASTM D638
Tensile Modulus 860000 psiASTM D638
Flexural Strength 19000 psiASTM D790
Flexural Modulus 798000 psiASTM D790
Izod Impact, Notched 1.50 ft-lb/inASTM D256
Coefficient of Friction, Dynamic 0.2240 psi, 50 fpm; ASTM D3702
K (wear) Factor 120 x 10-10 in³-min/ft-lb-hr40 psi, 50 fpm; ASTM D3702
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+17 ohm-cmASTM D257
Dielectric Constant 3.13
@Frequency 1e+6 Hz
ASTM D150
 3.17
@Frequency 60 Hz
ASTM D150
Dielectric Strength 490 V/milASTM D149
Dissipation Factor 0.00090
@Frequency 60 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 15.0 µin/in-°F
@Temperature 20.0 °C
ASTM D696
Maximum Service Temperature, Air 266 °FLong Term; ASTM UL746B
 270 °FIntermittent
Deflection Temperature at 0.46 MPa (66 psi) 298 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 295 °FASTM D648
Vicat Softening Point 329 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Delrin Delrin® 570 NC000 POM-GF20
AK Steel ZINCGRIP® GA Hot Dip Galvannealed Carbon Extra Deep Drawing Steel (EDDS), Standard Grade
AISI 5160 Steel, oil quenched from 830°C (1525°F), 650°C (1200°F) temper, 25 mm (1 in.) round
Aluminum 380.0-F Die Casting Alloy
Aluminum 5052-H32

PENS93 / 36002

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.