PPS-SGRN10 is a PPS resin of linear structure with narrow molecular weight distribution, we can provide consistently different grades of products which MFR from 120-200 g/10min. PPS-SGRN10 grade PPS resin could be used for spinning. Applications: Due to its high performance, PPS-SGRN10grade PPS resin is widely used in spinning industry. For example, dust bag with high-temperature corrosion resistance, non-woven. Information provided by Shandong Sciengy New Materials Co. Ltd |