Design/Construction:- Interleave 1: LDPE
- Side 1 Layer 2: Uncured Silicone Rubber
- Side 1 Layer 1: Cured Silicone Rubber
- Substrate: Style 1165 Fiberglass
- Side 2: Uncured Silicone Rubber
- Interleave: LDPE
UL Recognition File E54153 Information provided by Arlon Silicone Technologies Division; now a part of Rogers Corporation. |