MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Baystar™ 50100.2 HDPE blow molding, sheet, thermoforming resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Blow Molding Grade

Material Notes: Characteristics:
  • Good melt strength
  • Excellent stress cracking resistance
  • Good rigidity
  • Excellent impact strength
Applications:
  • Industrial parts
  • Jerry cans
  • Pallets
  • Large foamed parts
  • Suitable for food packaging
  • Toys
  • Sheet

This former Total Petrochemicals grade is now a part of the Bayport Polymers joint venture.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.950 g/ccASTM D-792
ESCR 100% Igepal® >= 600 hourASTM D1693, B
ESCR 10% Igepal® 120 hourASTM D1693, B
High Load Melt Index 10 g/10 min
@Load 21.6 kg,
Temperature 190 °C
ASTM D-1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 3800 psiASTM D-638
Elongation at Break >= 600 %ASTM D-638
Flexural Modulus 175 ksiASTM D-790
Izod Impact, Notched 10.0 ft-lb/inASTM D-256
 
Thermal PropertiesOriginal ValueComments
Melting Point 260 °FASTM D-3417

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for High Density Polyethylene (HDPE), Sheet/Thermoforming Grade
Overview of materials for High Density Polyethylene (HDPE), Injection Molded
Buckeye Polymers BP FLEX D6020-08 BLK Thermoplastic Polyolefin
Borealis BL2571 High Density Polyethylene

PBAYST806 / 38638

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.