MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Borealis Borstar® HE3492-LS Yellow-Orange High Density Polyethylene for Natural Gas Pipes  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Pipe Grade

Material Notes: Borstar HE3492-LS is a yellow-orange, cadmium free, high density polyethylene compound classified as a MRS 10.0 material (PE100) produced with the advanced Borstar technology. It includes a combination of pigments and stabilizers to ensure long-term, UV-resistance, and resistance to gas condensate. It also shows excellent resistance to rapid crack propagation and slow crack growth.

Borstar HE3492-LS is recommended for pressure pipe systems in the applications field of drinking water and natural gas, and gives good processing properties and low sagging in thick-walled pipes.

Information provided by the Manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.951 g/ccCompound; ISO 1183
Environmental Stress Crack Resistance >= 1000 hour
@Temperature 80.0 °C
At 9.2 bar; ISO 13479
Melt Flow 0.30 g/10 min
@Load 5.00 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 3625 psiAt 50 mm/min; ISO 527-2
Elongation at Break >= 600 %ISO 527-2
Tensile Modulus 1.10 GPaAt 1 mm/min; ISO 527-2
 
Processing PropertiesOriginal ValueComments
Front Barrel Temperature 190 - 210 °C
Die Temperature 392 - 410 °F
Melt Temperature 200 - 220 °C
Head Temperature 200 - 210 °C
 
Descriptive Properties
Resistance to Rapid Crack Propagation, BAR10ISO 13477, Pc at 0°C, S4 / pipe size 250 mm SDR 11

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for High Density Polyethylene (HDPE), Pipe Grade
Total XSene® XRC 20 B High Density Polyethylene - Pipes and Fittings
Borealis BorSafe™ HE3490-LS Black High Density Polyethylene for Pressure Pipes
Borealis BorPEX™ HE2557 Yellow High Density Polyethylene Compound for Crosslinked Pipes (Pex-A (Peroxide))
Borealis BorSafe™ HE3470-LS Black HDPE Compound for Pressure Pipes

PBOREA122 / 27429

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.