Moplen EP548U is a nucleated heterophasic copolymer with antistatic activation, used in injection molding applications. It exhibits an good impact/stiffness balance combined with a high fluidity. Moplen EP548U is typically used in opaque containers, house wares, toys and in thin-walled containers for food packaging (e.g. margarine tubs, yoghurt pots, etc.). Applications: House wares, Opaque Containers, Sports, Leisure & ToysInformation provided by LyondellBasell. |