MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

(Viewing data as-entered. Click here to return)
ATI Allegheny Ludlum AL 276™ Nickel-Base Alloy, UNS N10276
Categories: Metal; Nonferrous Metal; Nickel Alloy; Superalloy

Material Notes: AL 276 alloy is a nickel-chromium-iron-tungsten alloy which is among the most corrosion resistant of alloys currently available. The AL 276 alloy is widely used in the severest environments encountered in the chemical and petrochemical processing, flue gas desulfurization, pulp and paper and other specialized fields. Design of the alloy allows a high level of corrosion resistance to be retained even in the welded condition.

This alloy also has good high temperature strength and moderate oxidation resistance although the alloy will eventually form embrittling high temperature precipitates. It has been available for several years and has been used in ASME Boiler and Pressure Vessel related construction. The alloy is readily fabricated by welding using techniques similar to those used for austenitic stainless steels and other nickel base alloys. Precautions are advisable during fabrication because raising the low carbon and silicon contents of the material may adversely affect important properties.

Information provided by Allegheny Ludlum

Key Words: DIN 2.4819; ASTM B-575; ASME SB-575
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 8.90 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B <= 100
Tensile Strength, Ultimate >= 690 MPa
Tensile Strength, Yield >= 283 MPa
@Strain 0.2 %
Elongation at Break >= 40 %in 2"
Modulus of Elasticity 205 GPa
Charpy Impact 325 J10 mm sample from annealed plate
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.000130 ohm-cm
Magnetic Permeability 1.02
 
Thermal PropertiesOriginal ValueComments
CTE, linear 11.2 µm/m-°C
@Temperature 20.0 - 93.0 °C
 12.8 µm/m-°C
@Temperature 20.0 - 315 °C
 13.4 µm/m-°C
@Temperature 20.0 - 538 °C
Specific Heat Capacity 0.425 J/g-°C
Thermal Conductivity 10.2 W/m-K
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.0040 %
Chromium, Cr 15.5 %
Cobalt, Co 0.10 %
Iron, Fe 6.0 %
Manganese, Mn 0.15 %
Molybdenum, Mo 16 %
Nickel, Ni 59 %as balance
Phosphorus, P 0.0050 %
Silicon, Si 0.030 %
Sulfur, S 0.0020 %
Tungsten, W 3.5 %
Vanadium, V 0.15 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Special Metals INCONEL® Alloy C-276
ATI Allegheny Ludlum Grade 3 Titanium (UNS R50550)
ATI Allvac® Nickelvac® H-W Nickel Superalloy, Heat Treatment: 1185°C (2165°F) Anneal
Special Metals Nickel 200
Eagle Brass 519 Phosphor Bronze 6%, Extra Hard

NLN276 / 18013

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.