MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chemical Concepts Adhesive Ways 300M Synthetic elastomer contact bond adhesive
Categories: Polymer; Adhesive; Thermoset

Material Notes: A non-flammable high solids synthetic elastomer contact bond adhesive specifically formulated for bonding various types of polystyrene foams and plastic laminates to plywood and aluminum skins for recreational vehicles, mobile homes, modular panels and carpeting for boats and pool decking. Excellent spray break up and fluid distribution rates, which will not attack foam. Substrates should be under at least 20 psi or more if available within the limitations of the substrate. Adhesive coat should be dry (normally 2-5 mins. dry time is sufficient). Cure: 90% within 12 hours and full strength within 2-3 days. High resistance to water, humidity and alcohol. Allows immediate machining – after at least 20 psi of pressure between the two substrates to be bonded. High heat, creep and dead load resistance.

Information provided by Chemical Concepts™.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 27 %27 %+-1%
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
Appearancesyrup consistency
Odoramber or red
Tack Free Time15 seconds
Weight9.9 lb/gal

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ovako 42NiSiCrMo8-7-3* 497Q Steel, Quenching
AISI 4340 Steel, oil quenched 845°C, 425°C (800°F) temper
ATI Allvac® Vasco® 4340 Specialty Steel, Heat Treatment: 899°C (1650°F) Q+T
AISI 4340 Steel, oil quenched 800°C (1470°F), 540°C (1000°F) temper, 13 mm (0.5 in.) round
AISI 4340 Steel, oil quenched 800°C (1470°F), 595°C (1100°F) temper, 13 mm (0.5 in.) round

PCHEMI900 / 232225

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.