ULTEM™ AMHU1010F filament is a polyetherimide product for 3D printing applications manufactured fromULTEM™ HU1010 resin. The filament is biocompatible (ISO 10993 or USP Class VI) and printed parts can be gamma, EtO or steam sterilized. This filament can be used for food and drug packaging and medical device manufacturing, from conceptual modeling to functional prototyping and end-use parts. Filament spools can be linked to resin raw material batch to help ensure material compliance and traceability.*
*It is the responsibility of the finished device manufacturer to determine the suitability of all the component parts and materials used in their finished products. SABIC does not recommend and will not support the use of any of SABIC’s products in medical devices intended to remain continuously in the human body for longer than 29 days. Information provided by SABIC |