MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BJB Enterprises WC-595 A/B Clear Aliphatic Polyurethane Elastomer
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Elastomer, Unreinforced

Material Notes: WC-595 A/B is a two-part, clear, 90 Shore A polyurethane elastomer. It is recommended for use wherever a tough, flexible, permanently transparent elastomer is required. It is UV light and oxidation resistant and can be easily tinted or pigmented to clean bright colors. WC-595 A/B does not contain MOCA, MDA or TDI. In addition to being an excellent cast able product, it also functions well as an adhesive for bonding various substrates.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.03 g/cc1.03 g/ccPart B
 1.07 g/cc1.07 g/ccPart A
Density 1.03 g/cc0.0372 lb/in³ASTM D792
Brookfield Viscosity  350 cP
@Temperature 25.0 °C
350 cP
@Temperature 77.0 °F
Part B
 900 cP
@Temperature 25.0 °C
900 cP
@Temperature 77.0 °F
Mixed Part A & Part B
 2400 cP
@Temperature 25.0 °C
2400 cP
@Temperature 77.0 °F
Part A
Linear Mold Shrinkage 0.0050 cm/cm0.0050 in/inASTM D2566
Storage Temperature 18.3 - 26.7 °C65.0 - 80.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 85 - 9585 - 95ASTM D2240
Tensile Strength 27.6 MPa4000 psiASTM D412
Elongation at Break 180 %180 %ASTM D412
Tear Strength 65.7 kN/m375 pliASTM D624
 
Processing PropertiesMetricEnglishComments
Processing Temperature <= 93.3 °C<= 200 °FMax cure temp.
Cure Time  60.0 - 180 min
@Temperature 25.0 °C
1.00 - 3.00 hour
@Temperature 77.0 °F
Step 1 recommended high temp cure (as tested).
 960 min
@Temperature 71.1 °C
16.0 hour
@Temperature 160 °F
Step 2 recommended high temp cure (as tested).
 7200 - 10100 min
@Temperature 25.0 °C
120 - 168 hour
@Temperature 77.0 °F
Optional low temp cure
Working Life 15.0 min
@Temperature 25.0 °C
15.0 min
@Temperature 77.0 °F
100 g.
Gel Time 20.0 min20.0 min
Shelf Life 6.00 Month6.00 MonthStored at recommended temperatures. Purge opened containers with dry nitrogen before resealing.
 
Descriptive Properties
Color / AppearanceColorlessPart A
 ColorlessPart B
 Colorless/clearCured
Demold Time (hrs)6¼” thick; 4 hours in larger mass. @ 77°F
Mix Ratio by volume100 to 93Part A to Part B.
Mix Ratio by weight100 to 90Part A to Part B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBJB9924 / 287704

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.