MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 60 PHR N330 (HAF) Black
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Elastomer, Unreinforced; Rubber or Thermoset Elastomer (TSE)

Material Notes: MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is carried out by the use of various peroxides including dicumyl peroxide (DCP) or 2,5-dimethyl-2,5-bis (t-butylperoxy) hexane (DBPH).

All information provided by TSE Industries

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8484heat aged one week at 300ºF
 8686
 8989heat aged 70 hours at 300ºF
Tensile Strength 10.3 MPa1500 psiheat aged one week at 300ºF
 14.5 MPa2100 psiheat aged 70 hours at 300ºF
 24.9 MPa3610 psi
Elongation at Break 220 %220 %heat aged 70 hours at 300ºF
 230 %230 %heat aged one week at 300ºF
 280 %280 %
100% Modulus  4.83 MPa
@Strain 100 %
700 psi
@Strain 100 %
heat aged one week at 300ºF
 6.55 MPa
@Strain 100 %
950 psi
@Strain 100 %
heat aged 70 hours at 300ºF
 9.93 MPa
@Strain 100 %
1440 psi
@Strain 100 %
200% Modulus  7.93 MPa
@Strain 200 %
1150 psi
@Strain 200 %
heat aged one week at 300ºF
 13.1 MPa
@Strain 200 %
1900 psi
@Strain 200 %
heat aged 70 hours at 300ºF
 20.7 MPa
@Strain 200 %
3000 psi
@Strain 200 %
 
Processing PropertiesMetricEnglishComments
Cure Time 30.0 min
@Temperature 152 °C
0.500 hour
@Temperature 305 °F
 
Descriptive Properties
Formulation as Tested0.25Stearic Acid
 100Millathane 5004
 5.3Di-Cup 40C
 60N330 (HAF) Black

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMILL355 / 87399

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.