MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Kuraray HYBRAR® HD3 Thermoplastic Rubber-HDPE Blend
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Elastomer, Melt-Processible Rubber; Polyethylene (PE); High Density (HDPE)

Material Notes: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubber which exhibits high vibration damping properties at room temperatures. Both hydrogenated and non-hydrogenated grades of HYBRAR® are available. In addition to the superior vibration damping properties, hydrogenated grades also exhibit excellent miscibility with polypropylene, and may be used to produce blends with excellent transparency, flexibility and mechanical properties.

Blends of HYBRAR® and other polymers exhibit excellent vibration damping properties.

Mixing Conditions: Brabender Plasticorder @ 200°C

Molding Conditions: Press Molding @ 210°C

Formulation (parts by weight): High Density Polyethylene - 90, HYBRAR® 5127 - 10

Information provided by The Kuraray Group.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 58
Tensile Strength, Ultimate 25.0 MPa
Tensile Strength, Yield 47.0 MPa
Elongation at Break 1655 %
Tensile Modulus 0.853 GPa
 
Descriptive Properties
Viscoelasticity Loss Factor0.077at 40°C, measured w/ Rheovibron @ 110 Hz
Viscoelasticity; Tan Delta0.036measured by resonance method with a cantilever beam
 0.07at 0°C, measured w/ Rheovibron @ 11 Hz
 0.072at 25°C, measured w/ Rheovibron @ 110 Hz

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Kuraray HYBRAR® Low Rebound Compound # 1
Kuraray HYBRAR® HD2 Thermoplastic Rubber-HDPE Blend
Kuraray SEPTON® CM1 Compatibilizer
Kuraray SEPTON® H5127
Kuraray HYBRAR® F1 Foam Compound

PKUR040 / 49429

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.